Specification & Parameter | ||||||||||
Specification | 18 Gloss | 21 Gloss | 24 Gloss | 27 Gloss | 18 Matt | 21 Matt | 24 Matt | 27 Matt | ||
Thickness | BASE | 12 | 12 | 15 | 15 | 12 | 12 | 15 | 15 | |
EVA | 6 | 9 | 9 | 12 | 6 | 9 | 9 | 12 | ||
TOTAL | 18 | 21 | 24 | 27 | 18 | 21 | 24 | 27 | ||
Width | 200mm-1890mm, Upon customer's requitement | |||||||||
Length | 200-6000 more or less 10% allowed | |||||||||
CoronaTreatment Side | A(Surface) | B(EVA side) | AB(Both side) | |||||||
Peper Corelinter Dia | 25.4mm(1')/76mm(3')/155mm(6') |
PHOTO ALBUM, POSTER, PAPER BAG, BOOKS COVERS, MAGAZINES, CATALOGS, OUTDOOR ADVERTISEMENT, LABELS, CARTON,BOX
Benzene X Bubble X Peeling X
Environmentally-friendly V Energy efficient V
High moisture content and bigger size paper, or digital prints, advertising inject prints
▎Please adjust the pressure and temperature according to different types of paper and ink.
▎When using the film for the first time, or changing to other sizes or printing materials, please get a small trial volume before going into fully mass lamination.
▎The following situation will affect the quality of the film during lamination.
◆ The ink contains too much wax, dried oil, adhesive, and silicon additive .etc.
◆ using metal ink or the ink is too thick
◆ the ink is not totally dry
◆ the paper is high humidity
◆ there is too much powder
◆ tension setting is not correct on laminators
◆ relevant technical support on after-seals process
● Coating EVA
● On-line thickness gauge measuring
● Curing process of EVA( Solidification Ripening)
● Sliting into different size, rewingding in smooth roll